Chapter 25-2, Residual stress, china injection mold
Unbalanced cooling from the mold wall to its center can cause thermal-induced residual stress. Furthermore, asymmetrical thermal-induced residual stress can occur if the cooling rate of the two surfaces is unbalanced. Such unbalanced cooling will result in an...
Chapter 25-3, Residual stress, china injection mold
Chapter 25-3, Residual stress, china injection mold Home » Mould Technology Blog » News Center » Chapter 25-3, Residual stress, china injection mold FIGURE 5. Variable residual stresses arise and the part deforms as layers of different frozen-in specific volume...
Chapter 26-1,Shrinkage and warpage
Why do they occur? Shrinkage is inherent in the injection molding process. Shrinkage occurs because the density of polymer varies from the processing temperature to the ambient temperature (see Specific volume (pvT diagram)). During injection molding, the variation in...
china mold company ‘s chance
china mold company ‘s chance Home » Mold Industry Blogy » News Center » china mold company ‘s chance In order to produce injection molding processors can save costs and time , and improve production efficiency injection mold, mold manufacturers increasing use of new...
Home appliance mold industrial status
Home appliance mold industrial status “Mould is the foundation of all industrial.” said to the media by Mr.WU , the CEO of the China Die & Mould Industry Association. nowdays, electronics, automotive, electric machine, electrical appliance, instrument, home...
Compare the superiority of major mould manufacturing countries
Compare the superiority of major mould manufacturing countries Home » Mold Industry Blogy » News Center » Compare the superiority of major mould manufacturing countries The world’s major manufacturering countries, including the Asian region :Japan, South Korea and...
The cause to be a successful plastic injection factory
The cause to be a successful plastic injection factory Always I got auction notices in private email inbox, and staring at the photographs of the shops that are going out of business, you were wondering: What does it turn to be a perfect plastic injection...
China’s steel industry to face tougher times in 2011
China’s steel industry to face tougher times in 2011 BEIJING, Feb. 16 (Xinhua) — China’s steel companies will come under pressure this year as the government restructures the economy and competition heats up on the global market, said a report released Wednesday by...
Mold Product
→ MOLD
→ Prototype parts
→ Plastic Part
→ silicone & rubber parts
Contact Us
DONGGUAN SINCERE TECH CO.LTD
FACTORY ADDRESS: YUANXIA LU, YUANJIANG YUANG, CHANGPING TOWN, DONNGUAN CITY,GUANGDONG PROVINCE, CHINA 523000
TEL: +86 (0)769 3366 9997
FAX: +86 (0)769 3366 9997
EMAIL: INFO@sinceretetechs.com

Chapter 25-2, Residual stress, china injection mold
Unbalanced cooling from the mold wall to its center can cause thermal-induced residual stress. Furthermore, asymmetrical thermal-induced residual stress can occur if the cooling rate of the two surfaces is unbalanced. Such unbalanced cooling will result in an...
Chapter 25-3, Residual stress, china injection mold
Chapter 25-3, Residual stress, china injection mold Home » Mould Technology Blog » News Center » Chapter 25-3, Residual stress, china injection mold FIGURE 5. Variable residual stresses arise and the part deforms as layers of different frozen-in specific volume...
Chapter 26-1,Shrinkage and warpage
Why do they occur? Shrinkage is inherent in the injection molding process. Shrinkage occurs because the density of polymer varies from the processing temperature to the ambient temperature (see Specific volume (pvT diagram)). During injection molding, the variation in...
china mold company ‘s chance
china mold company ‘s chance Home » Mold Industry Blogy » News Center » china mold company ‘s chance In order to produce injection molding processors can save costs and time , and improve production efficiency injection mold, mold manufacturers increasing use of new...
Home appliance mold industrial status
Home appliance mold industrial status “Mould is the foundation of all industrial.” said to the media by Mr.WU , the CEO of the China Die & Mould Industry Association. nowdays, electronics, automotive, electric machine, electrical appliance, instrument, home...
Compare the superiority of major mould manufacturing countries
Compare the superiority of major mould manufacturing countries Home » Mold Industry Blogy » News Center » Compare the superiority of major mould manufacturing countries The world’s major manufacturering countries, including the Asian region :Japan, South Korea and...
The cause to be a successful plastic injection factory
The cause to be a successful plastic injection factory Always I got auction notices in private email inbox, and staring at the photographs of the shops that are going out of business, you were wondering: What does it turn to be a perfect plastic injection...
China’s steel industry to face tougher times in 2011
China’s steel industry to face tougher times in 2011 BEIJING, Feb. 16 (Xinhua) — China’s steel companies will come under pressure this year as the government restructures the economy and competition heats up on the global market, said a report released Wednesday by...
China plastic injection mold, toolmaker, China mould maker, China tooling, Plastic mould china, China injection mold factory, plastic injection mold manufacturer in china
Copyright © 2011 DONGGUAN SINCER TECH CO.LTD. | China Mold maker, china Plastic injection molding, china toolmaker.
Company Register No.:1626173