Plastic injection molding process

we are very professinoal plastic injection molding company in china,So I would love to introduce you the process of plastic injection molding.

All of this resin material started out generally as plastic pellets. The pellets are feed into one of the massive injection molding machines, these injection machines often weigh around 25 tons. The machine heats the plastic until it is liquid. This liquid is then forced through injectors into injection molds.

These injection molds can be made to almost any shape or size. To put it simply, injection molding is the process of forcing melted plastic in to a mold cavity. Once the plastic has cooled, the part can be ejected out. It is useful when the parts are too complex or cost prohibitive to machine. With this process, many parts can be made at the same time, out of the same plastic injection mold.

The process has normally six steps:

1. Clamping: the injection machine has three parts. The injection mold, the clamp and the injection unit. The clamping unit holds the mold at a certain pressure, this ensures uniformity in the units that are outputted.

Molds are normally made from two parts.

2. Injection Unit: this is where the plastic pellets are loaded into a hopper at the top of the injection unit. The pellets are fed into the main cylinder; this is where they are heated until they are liquefied. Inside the injection unit there is a screw which turns and mixes the plastic. Once this liquid plastic has reached the optimum for this product the injection process starts. The plastic is forced through a sprue and the pressure and speed are controlled by the screw or sometimes a ram depending on the type of machine.

3. Dwelling: this is a pause in the process while some pressure is applied to ensure all the mold cavities have been completely filled. This is very important within the process as it will result in a scrap of units if the mold is not filled correctly.

4. Cooling: this part of the process lets the mold cool for the required period. If it is done too quickly the units can stick or become deformed once out of the machine.

5. Mold Opens: The clamping unit is opened to separate the mold. Molds are used over and over again; they are often the most important single part in the whole process. The tooling of mold can be very expensive.

6. Ejection: the finished product is ejected from the injection mold machine. Often the finished product will continue on a production line or be stacked to go to a production line as parts for larger products, e.g. car steering wheel.

The products that use injection molding are used every day by all of us. Many cars would not be so affordable if it was not for injection molding, however, there are some disadvantages to the process. The machinery is very expensive and involves high capital investment, design of parts must bear in mind the production process, and the process is not economically for short runs of products.

However the disadvantage is out-weighed by the greater advantages, the speed at which parts can be made, low labor costs, minimal material waste, and finished parts often need no more finishing.

if you interest in our service or need some technical support, please feel to contact us, also we can share what we know about plastic injection molding and provide some economic plastic injection molding solution.